System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Kuraray Genestar™ GN2330 Nylon, 33% Glass Filled
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
Material Notes:
Standard V-0 Grade. Features a balance of mechanical strength, mold-ability, and dimensional stability. Well suited for a wide range of electrical and electronic components.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.62
g/cc
1.62
g/cc
Water Absorption
1.0 %
1.0 %
Linear Mold Shrinkage, Flow
0.0010
cm/cm
0.0010
in/in
Linear Mold Shrinkage, Transverse
0.0060
cm/cm
0.0060
in/in
Melt Flow
21
g/10 min
@Load 2.16 kg,
Temperature 320 °C
21
g/10 min
@Load 4.76 lb,
Temperature 608 °F
ASTM D1238
Spiral Flow
5.50
cm
@Load 750 kg,
Temperature 320 °C
2.17
in
@Load 1650 lb,
Temperature 608 °F
0.5mm diameter
Mechanical Properties
Metric
English
Comments
Tensile Strength
54.0
MPa
7830
psi
Weld; ASTM D638
185
MPa
26800
psi
ASTM D638
Elongation at Yield
0.70 %
0.70 %
Weld; ASTM D638
4.0 %
4.0 %
ASTM D638
Flexural Strength
240
MPa
34800
psi
ASTM D790
Flexural Modulus
11.0
GPa
1600
ksi
ASTM D790
Izod Impact, Notched
1.00
J/cm
1.87
ft-lb/in
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+16
ohm-cm
1.00e+16
ohm-cm
ASTM D257
Dielectric Constant
3.4
@Frequency 1e+10 Hz
3.4
@Frequency 1e+10 Hz
ASTM D150
Dielectric Strength
30.0
kV/mm
762
kV/in
ASTM D149
Dielectric Loss Index
0.010
@Frequency 1e+10 Hz
0.010
@Frequency 1e+10 Hz
ASTM D150
Comparative Tracking Index
400
-
600
V
400
-
600
V
ASTM UL746A
Thermal Properties
Metric
English
Comments
Melting Point
306
°C
583
°F
Deflection Temperature at 1.8 MPa (264 psi)
285
°C
545
°F
ASTM D648
Glass Transition Temp, Tg
125
°C
257
°F
Flammability, UL94
V-0
V-0
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Kuraray Genestar™ GR2300 Nylon, 30% Glass Filled
Kuraray Genestar™ GN2450 Nylon, 45% Glass Filled
Kuraray Genestar™ GW2458HF Nylon, 45% Glass Filled
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM)
Celanese Zytel® HTNFR52G30NH NC010 PA6T/66-GF30FR(40)
PKUR121 / 162510
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.