MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sax Polymers SAXAMID 126F6 Nylon 6, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: SAXAMID 126F6 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Other properties are very good processability and good surface quality.

Information provided by SAX Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Viscosity Test 150 cm³/g1.50 dl/gH2SO4; ISO 307
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 190 MPa27600 psi5 mm/min; ISO 527-1
Elongation at Break 4.0 %4.0 %5 mm/min; ISO 527-1
Tensile Modulus 9.20 GPa1330 ksi1 mm/min; ISO 527-1
Flexural Strength 280 MPa40600 psi2 mm/min; ISO 178
Flexural Modulus 7.60 GPa1100 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  78.0 kJ/m²
@Temperature -30.0 °C
37.1 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1U
 82.0 kJ/m²
@Temperature 23.0 °C
39.0 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched  8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 209 °C408 °F80*10*4 s=60mm; ISO 75-1 a
Vicat Softening Point 216 °C421 °FB/120; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 80.0 °C
@Time 7200 - 21600 sec
176 °F
@Time 2.00 - 6.00 hour
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sax Polymers SAXAMID 126 Nylon 6, Injection Molding Grade

PSAXP936 / 150885

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.