MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Reynolds TASK® 8 Heat Resistant Polyurethane Resin
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: TASK™ 8 is a heat resistant polyurethane resin system made specifically for prototyping / casting applications which require thermal resistance of up to 263°F /129°C. TASK™ 8 offers the convenience of a 1A:1B mix ratio and has a very low viscosity, so it is easy to mix and pour. Plastic cures quickly to a Shore 80D and exhibits good physical and performance properties. Heat curing this material is necessary to attain optimal heat resistance. See “Heat Curing” section for curing schedule details. Applications include making machine housings, thermo-forming and general prototyping / casting.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D-1475
Viscosity 100 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.010 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D-2240
Tensile Strength, Ultimate 5840 psiASTM D-638
Elongation at Break 4.0 %ASTM D-638
Tensile Modulus 246000 psiASTM D-638
Flexural Strength 8280 psiASTM D-790
Flexural Modulus 271000 psiASTM D-790
Compressive Strength 8760 psiASTM D-695
Compressive Modulus 77400 psiASTM D-695
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 90.0 °CAfter Heat Curing; ASTM D-648
 129 °CAfter 1 Week At 73°F/23°C; ASTM D-648
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 15.0 minHandling Time
Pot Life 2.50 minASTM D-2471
 
Descriptive Properties
ColorOff-White
Mix Ratio120A:100Bby weight
 1A:1Bby volume
Specific Volume25.4[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN035 / 296736

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.