Dry as molded. Nylene NX1731 is a general purpose grade nylon 6 resin which is suitable for molding or extrusion. It is recommended for industrial applications where the toughness, chemical
resistance, and high temperature properties of nylon 6 are required but where some color
variation is acceptable. Optimum processing conditions should provide a melt temperature of
480 - 500ºF at the die or nozzle. Data provided by the manufacturer |