MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SCG Chemicals C2670XXX PVC Wire & Cable Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: C2670XXX is PVC compound product with any color for using in wire and cable application product. The formulation is designed Cable Tape and Non heavy metal which give good process ability by Calendaring.

Applications: PVC CABLE TAPE.

Features: Good process ability. Good surface product. Non heavy metal.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 - 1.32 g/cc1.29 - 1.32 g/ccJIS K7112
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 72 - 77
@Time 10.0 sec
72 - 77
@Time 0.00278 hour
JIS K6253
Tensile Strength 15.0 - 16.0 MPa2180 - 2320 psiJIS K6723
Elongation at Break 291 - 392 %291 - 392 %JIS K6723
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+12 - 1.65e+13 ohm-cm3.00e+12 - 1.65e+13 ohm-cmJIS K6723
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -25.0 °C-13.0 °FJIS K6723
 
Descriptive Properties
AppearancePellet
BleedingNot bleedingTPC Method
Heat Stability80-265 minJIS K6723 @ 180°C
Retention of Elongation at Break (%)86-96JIS K6723. Aging @ 80°C x 168 hrs.
Retention of Tensile Strength (%)102-108JIS K6723. Aging @ 80°C x 168 hrs.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC788 / 278045

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.