MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 2099 X 134514 C Polycarbonate/PBT Alloy (PC/PBT), High Impact - Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled; Polyester, TP; Polybutylene Terephthalate (PBT)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.28 g/ccASTM D 792
Linear Mold Shrinkage 0.0060 - 0.0090 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9500 psiASTM D 638
Elongation at Break >= 10 %ASTM D 638
Tensile Modulus 350 ksiASTM D 638
Flexural Strength 15500 psiASTM D 790
Flexural Modulus 400 ksiASTM D 790
Izod Impact, Notched 10.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
ASTM D 4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 200 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
 5VA
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 470 - 540 °F
Mold Temperature 140 - 200 °F
Drying Temperature 180 - 220 °F
@Time 14400 sec
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade
Ravago Manufacturing Americas Hybrid B2035I PC/PBT Impact Resistant, High Flow, DAM
Ravago Manufacturing Americas Hybrid B2026I PC/PBT, Impact Resistant, DAM
Eurotec® Tecodur® PB70 NL TD22 PBT/PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural
Covestro Makroblend® KU 2-7609 Polycarbonate + PBT, Mineral Filled Impact Grade

PQZQA31971 / 239922

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.