Toray CFRT® NRG Plates are used in medical applications to limit motion such as with Turf Toe or Hallux Rigidus and partial foot amputations. They are also used to make improvements in patients’ gait and to redistribute pressures to less sensitive areas of the foot for diabetic patients. Toray CFRT® NRG plates are thermoplastic composite laminates that are made using Toray Cetex® TC940, a semi-crystalline polyethylene terephthalate (PET) matrix resin. NRG Plates are available in Semi-Flex, Semi-Rigid, and Rigid grades and in various styles including Flat Plates, Contour Plates, and Morton Toe Plates. High performance, continuous Fiber Reinforced Thermoplastic construction providing high strength to weight ratio. - High resilience - will not lose shape or material properties after continued use in high loading applications.
- Easy to bond using conventional adhesives.
- Easy to fit and finish.
Information provided by Toray Performance Materials Corporation. |