MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker R2000/30 Silicone Rubber Base
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: R2000/30 Silicone Rubber Base is an all purpose base.

Special features:

  • Good balance of properties
  • Good compression set
  • Good molding qualities
  • Excellent shelf stability
  • Excellent filler acceptance

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3131ASTM D2240
Tensile Strength at Break 7.30 MPa1060 psiASTM D412
Elongation at Break 839 %839 %ASTM D412
Tear Strength 16.1 kN/m91.9 pliASTM D624
Compression Set 21 %
@Temperature 177 °C,
Time 79200 sec
21 %
@Temperature 351 °F,
Time 22.0 hour
Method B; WSTM 1114
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min
@Treatment Temp. 171 °C
0.167 hour
@Treatment Temp. 340 °F
press cured
 
Descriptive Properties
Appearancetranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® R plus 533/60 A/B Silicone Rubber

PWACK9249 / 204778

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.