MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Syncon® FG Hydraulic Fluid ISO Grade 68
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Syncon FG Hydraulic Fluid is a premium quality, synthetic, food-grade antiwear hydraulic fluid developed for use in the hydraulic systems of machinery found in food processing plants and beverage bottling plants, where incidental food contact may occur. It also is recommended for use in rotary screw and rotary vane air compressors in food and beverage plants. Syncon FG Hydraulic Fluid is formulated with synthetic polyalphaolefin (PAO) base oils and an ashless (zinc-free) additive package to provide excellent service in hydraulic system applications. It provides excellent wear protection for hydraulic pumps and motors, and protects hydraulic system components against rust and corrosion. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It also has excellent low-temperature properties for cold start-ups. It has good water-separating properties to minimize the formation of emulsions, and is resistant to excessive foaming that can cause poor or sluggish hydraulic system response. Syncon FG Hydraulic Fluid meets FDA requirements and former 1998 USDA H1 guidelines for incidental food contact, and is registered by NSF International as an H1 lubricant. It meets the performance requirements of all major hydraulic pump manufacturers, and is recommended for use in all types of high-pressure, high-speed hydraulic pumps.

Applications:

  • Bottling and canning machines
  • Plastic injection blow-molding machines in food packaging plants
  • Rotary screw and rotary vane air compressors
  • Chain drives for conveyor belts
  • Electric motor bearings
  • Machinery operating in freezers used to store packaged food
Syncon FG Hydraulic Fluid meets the requirements of the following government and industry specifications:
  • FDA 21 CFR 178.3570 for incidental food contact
  • NSF International and former 1998 USDA H1 guidelines for incidental food contact
Features/Benefits:
  • Excellent wear protection for hydraulic pumps and motors
  • Outstanding oxidation resistance to minimize sludge and varnish formation
  • Protects against rust and corrosion
  • Good water-separating properties
  • Good foam resistance
  • Excellent low-temperature properties for cold start-ups

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.837 g/cc0.837 g/cc
Density 0.835 g/cc0.0302 lb/in³
Viscosity Measurement 133133Index
Saybolt Viscosity at 100°F 329 SUS329 SUS
Saybolt Viscosity at 210°F 59 SUS59 SUS
Kinematic Viscosity at 40°C (104°F) 64.2 cSt64.2 cSt
Kinematic Viscosity at 100°C (212°F) 9.7 cSt9.7 cSt
Oxidative Stability >= 28.33 hour>= 28.33 hourRPVOT; ASTM D2272
ASTM Color 0.500.50ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.670.67[mg KOH/g]; ASTM D974
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.370 mm0.0146 inScar Diameter; ASTM D4172
 
Thermal PropertiesMetricEnglishComments
Pour Point -48.0 °C-54.4 °F
Flash Point 252 °C486 °FCOC
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
USDA YesYes
 
Descriptive Properties
Copper Corrosion1aASTM D130
Demulsibility10 minutes to passASTM D1401
FZG Scuffing Test11 Failure Load StageASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5047 / 198300

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.