MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Shanghai Potomer ADC/S-C2 ADC blowing agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Easily dispersible, low-dust standard ADC, suitable for activation

Applications: ADC blowing agent is the most largest consumed chemical blowing agent in domestic market and it is widely used in blowing of PVC, PE, EVA, PP, PS, NR, ABS resin, nylon 66, CR, NBR, IIR, SBR, EPDM, silicon rubber and PVC/NBR blends both under normal and pressurized condition. It is suitable for blowing of close pore foams, normal pressure or pressurized foams and thick or thin foam. ADC is uniform in particle size, stable in quality and is suitable for high and middle class products which have high requirements on appearances and performances.

ADC blowing agent is in form of yellow power and its specific gravity is 1.65 and is non-poisonous, odorless and flammable. It is the most widely used organic chemical blowing agent. ADC has superior dispensability with large gas emission rate. The decompose gases are non-poisonous, odorless and pollution free. The main produced gas is nitrogen, which hardly comes out of the blown object. ADC is decomposed at 210-215? and its decomposition temperature can be lowered to 150-190? by addition of catalysts (like some of Zn-containing compounds) to get adapted to different requirement of different materials. Its decomposition temperature can be also lowered by addition of organic acids and their salts, urea, biuret, biurea, borax, ethanolamine, lead salts, etc. This can be considered in formula design.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.65 g/cc
Bulk Density 0.300 - 0.600 g/cc
Particle Size 5.7 - 7.7 µm
Specific Surface Area 3.2 - 3.8 m²/g
Molecular Weight 116.08 g/mol
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 215 °C
 
Descriptive Properties
Color/AppearanceYellow/crystalline power
Content(%)99ADC
Gas quantity220 ml/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSPOTOM002 / 284448

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.