MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BYK ADD-VANCE® THC 453 PP based masterbatch containing heat stabilizers and carbon black  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Stabilization masterbatch for producing long fiber reinforced polypropylene for D-LFT process
Examples: Long fiber reinforced pellets to be used for automotive parts, like underbody panels and shields, structural parts, etc.

Mode of action and advantages: ADD-VANCE® THC 453 contains a combination of heat stabilizers and carbon black. Heat stabilizers inhibit the thermo-oxidative degradation by radical scavenging and decomposing reactive hydroperoxides.

Advantages: Excellent Long Term Heat Ageing (LTHA) performance to achieve VW and D-C requirements. The minimum long term heat ageing will be 1200 hours @ 150°C applying 2 or 2,6% dosing level on PP, depending on the glass concentration; Excellent mechanical properties after heat-aging (D-C test method); Good glueing properties; High accuracy in dosing of each individual additive component in ADD-VANCE® THC 453 to ensure product consistency and a guaranteed stabilization of end-product; Optimized additive formulation to achieve lower overall additivation costs and easy processing; Non-sticking pellets, dust free dosing; and Safe and easy handling.

Former ADDCOMP product line, acquired by BYK.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.650 g/cc
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 300 °C
 
Descriptive Properties
AppearanceBlack granules
Dosing Level2%for LFT containing 20-30% glass
 2.6%for LFT containing 40% glass

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 2099 X 138797 Permanently Static Dissipative Masterbatch; ESD Protection
BYK ADD-VANCE® NU 489 Nucleation masterbatch, PP based
BYK ADD-VANCE® FR 243 Halogen-free flame retardant masterbatch, PP based
BYK ADD-VANCE® DS 785 Desiccant masterbatch in PP carrier
BYK ADD-MAX® AS 38 Anti-static masterbatch, LLDPE based

PPADDC28 / 133241

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.