MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Mineral/Glass Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 - 2.10 g/cc0.0560 - 0.0759 lb/in³Average value: 1.86 g/cc Grade Count:52
Water Absorption 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.0795 % Grade Count:40
Linear Mold Shrinkage 0.000600 - 0.00350 cm/cm0.000600 - 0.00350 in/inAverage value: 0.00199 cm/cm Grade Count:52
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 80.0 - 12380.0 - 123Average value: 96.0 Grade Count:14
Hardness, Rockwell M 107 - 120107 - 120Average value: 113 Grade Count:5
Tensile Strength, Ultimate 31.0 - 148 MPa4500 - 21500 psiAverage value: 91.4 MPa Grade Count:50
Elongation at Break 0.272 - 1.15 %0.272 - 1.15 %Average value: 0.565 % Grade Count:26
Modulus of Elasticity 9.50 - 30.0 GPa1380 - 4350 ksiAverage value: 20.0 GPa Grade Count:26
Flexural Yield Strength 60.0 - 249 MPa8700 - 36100 psiAverage value: 164 MPa Grade Count:52
Flexural Modulus 7.50 - 27.5 GPa1090 - 3990 ksiAverage value: 17.5 GPa Grade Count:50
Flexural Strain at Break 0.700 - 1.80 %0.700 - 1.80 %Average value: 0.984 % Grade Count:11
Compressive Yield Strength 145 - 410 MPa21000 - 59500 psiAverage value: 255 MPa Grade Count:45
Poissons Ratio 0.310 - 0.3300.310 - 0.330Average value: 0.317 Grade Count:3
Shear Modulus 5.46 - 5.98 GPa792 - 867 ksiAverage value: 5.76 GPa Grade Count:3
Izod Impact, Notched 0.163 - 0.558 J/cm0.305 - 1.05 ft-lb/inAverage value: 0.385 J/cm Grade Count:13
Charpy Impact Unnotched 0.400 - 1.50 J/cm²1.90 - 7.14 ft-lb/in²Average value: 0.887 J/cm² Grade Count:15
Charpy Impact, Notched 0.195 - 0.550 J/cm²0.928 - 2.62 ft-lb/in²Average value: 0.378 J/cm² Grade Count:48
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.90e+11 - 1.74e+15 ohm-cm1.90e+11 - 1.74e+15 ohm-cmAverage value: 1.47e+14 ohm-cm Grade Count:12
Insulation Resistance 2.00e+10 - 1.00e+14 ohm2.00e+10 - 1.00e+14 ohmAverage value: 3.85e+12 ohm Grade Count:21
Dielectric Constant 4.50 - 5.604.50 - 5.60Average value: 5.12 Grade Count:13
Dielectric Strength 8.60 - 35.0 kV/mm218 - 889 kV/inAverage value: 15.8 kV/mm Grade Count:36
Dissipation Factor 0.0120 - 0.2860.0120 - 0.286Average value: 0.0524 Grade Count:13
Arc Resistance 48.0 - 185 sec48.0 - 185 secAverage value: 154 sec Grade Count:20
Comparative Tracking Index 175 - 325 V175 - 325 VAverage value: 203 V Grade Count:25
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 - 38.0 µm/m-°C6.67 - 21.1 µin/in-°FAverage value: 19.1 µm/m-°C Grade Count:21
 49.0 - 75.0 µm/m-°C
@Temperature 40.0 - 130 °C
27.2 - 41.7 µin/in-°F
@Temperature 104 - 266 °F
Average value: 62.0 µm/m-°C Grade Count:2
CTE, linear, Transverse to Flow 20.0 - 45.0 µm/m-°C11.1 - 25.0 µin/in-°FAverage value: 28.1 µm/m-°C Grade Count:15
Thermal Conductivity 0.580 - 0.580 W/m-K
@Temperature 100 - 100 °C
4.03 - 4.03 BTU-in/hr-ft²-°F
@Temperature 212 - 212 °F
Average value: 0.580 W/m-K Grade Count:1
Maximum Service Temperature, Air 150 - 250 °C302 - 482 °FAverage value: 218 °C Grade Count:13
Deflection Temperature at 1.8 MPa (264 psi) 170 - 300 °C338 - 572 °FAverage value: 233 °C Grade Count:51
Deflection Temperature at 8.0 MPa 145 - 185 °C293 - 365 °FAverage value: 161 °C Grade Count:4
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Novolac, Glass Filled
Overview of materials for Phenolic, Resole, Glass Fiber Filled
Overview of materials for Phenolic/Glass Fiber SMC
Overview of materials for Phenolic, Ablative Coating
Sumitomo Bakelite FM 4004F Phenolic Novolac Compound

O2737 / 78100

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.