MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis OE5318I EVA Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: OE5318I is a copolymer of ethylene and vinyl acetate containing 18% vinyl acetate by weight.

Applications: OE5318I is intended for use in industrial applications but shall not be used for packaging.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³ISO 1183-1
Vinyl Acetate Content 18.0 %18.0 %
Melt Flow 2.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  91.0
@Time 15.0 sec
91.0
@Time 0.00417 hour
ISO 868
 92.0
@Time 1.00 sec
92.0
@Time 0.000278 hour
ISO 868
Hardness, Shore D  34.0
@Time 15.0 sec
34.0
@Time 0.00417 hour
ISO 868
 36.0
@Time 1.00 sec
36.0
@Time 0.000278 hour
ISO 868
Tensile Strength at Break 22.0 MPa3190 psi50 mm/min; ISO 527-2
 23.0 MPa3340 psi250 mm/min; ISO 527-2
Elongation at Break 826 %826 %50 mm/min; ISO 527-2
 840 %840 %250 mm/min; ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 86.0 °C187 °FISO 11357-3
Vicat Softening Point 58.0 °C
@Load 1.02 kg
136 °F
@Load 2.25 lb
A50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9852 / 323209

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.