MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite FM 4017F Phenolic Molding Compound
Categories: Polymer; Thermoset; Phenolic

Material Notes: FM 4017F is a fiberglass and mineral reinforced phenolic molding compound, with excellent dimensional stability and good strength at elevated temperatures.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.81 g/ccASTM D782
Apparent Bulk Density 0.800 g/ccPowder; ASTM D1895
Water Absorption 0.070 %
@Time 86400 sec
ASTM D570
 0.15 %
@Time 173000 sec
ASTM D570
Linear Mold Shrinkage 0.0020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 125ASTM D785
Tensile Strength 72.0 MPaASTM D638
Flexural Strength 135 MPaASTM D790
Flexural Modulus 15.0 GPaASTM D790
Compressive Strength 286 MPaASTM D695
Izod Impact, Notched 38.0 J/mASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 13.8 kV/mm
@Frequency 60 Hz
SS
 >= 14.8 kV/mm
@Frequency 60 Hz
ST
Arc Resistance 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 19.0 µm/m-°CASTM E831
Maximum Service Temperature, Air 150 °CUL 746B Temperature Index
Deflection Temperature at 1.8 MPa (264 psi) 190 °CAs Molded; ASTM D648A
 >= 282 °CPost Baked; ASTM D648A
Flammability, UL94 V-0
@Thickness 3.20 mm
 V-0
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUMIT161 / 193966

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.