MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2800 B-80A Z Thermoplastic Polyolefin Elastomer, FDA Compliant Ingredients  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Material Notes:


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccASTM D792
Linear Mold Shrinkage 0.015 - 0.019 cm/cm
@Thickness 3.17 mm
0.015 - 0.019 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 808010 sec; ASTM D2240
Tensile Strength at Break 6.89 MPa
@Thickness 3.17 mm
1000 psi
@Thickness 0.125 in
Die C, 20 in/min (500 mm/min); ASTM D412
Elongation at Break 650 %
@Thickness 3.17 mm
650 %
@Thickness 0.125 in
Die C, 20 in/min (500 mm/min); ASTM D412
Tear Strength 37.7 kN/m215 pliDie C; ASTM D624
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 171 - 210 °C340 - 410 °F
Mold Temperature 10.0 - 79.4 °C50.0 - 175 °F
Drying Temperature 79.4 °C175 °F3 - 4 hrs
Moisture Content <= 0.080 %<= 0.080 %
Injection Pressure 34.5 - 68.9 MPa5000 - 10000 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Elastamax™ XL-2065 Thermoplastic Polyolefin Elastomer (TPO (POE))
A. Schulman INVISION™ VX-5170UE Soft Touch Polyolefin Thermoplastic
RTP Company RTP 2800 B-75A Thermoplastic Polyolefin Elastomer (TEO)
RTP Company RTP 2800 D-75A Thermoplastic Polyolefin Elastomer (TEO)
RTP Company ESD A 2800 B-75A Black Thermoplastic Polyolefin Elastomer (TEO) ESD Protection - Static Dissipative

PQZXA7907 / 60228

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.