MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: An advanced composite formulated to protect concrete and metal surfaces from corrosion and chemical attack. It is normally applied at a thickness of 1-2 mm (40-80 mils) per coat. However, greater single coat film thickness is achievable when spray applied. Non-shrinking, 100% solids. ARC S1HB is a high viscosity, high performance composite lining that is designed to be a spray applied but may also be applied by brush. ARC S1HB allows for uniform coverage over rough surfaces and yields excellent immersion exposures. The cured ARC S1HB provides a barrier film with adhesion and resistance to corrosion.

Benefits:

  • High build capability for coverage over irregular surfaces.
  • Outlasts conventional paints and coatings
  • Long pot life allow for ease of use
  • 100% solids, no shrinkage on cure
  • Outstanding adhesion insures reliable performance
  • Able to be high voltage spark tested for pinhole free films.

Suggested Uses:

  • Bar Screen Chambers
  • Junction/Splitter Boxes
  • collection system Piping
  • Digesters
  • Sewer Piping
  • Waste water Clarifiers
  • Manholes
  • Thickener Tanks
  • ”Other” Concrete and Metal Structures

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccCured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ASTM D2240
Tensile Strength at Break 5610 psiASTM D638
Elongation at Break 6.0 %ASTM D638
Flexural Strength 8360 psiASTM D790
Flexural Modulus 430000 psiASTM D790
Compressive Strength 12390 psiASTM D695
Adhesive Bond Strength 1460 psiDry Concrete; ASTM D4541
 >= 2000 psiMetal; ASTM D4541
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 52.0 °CWet Service
 80.0 °CDry Service
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 hour
@Temperature 43.0 °C
Light Load
 16.0 hour
@Temperature 43.0 °C
Overcoat End
 18.0 hour
@Temperature 32.0 °C
Light Load
 24.0 hour
@Temperature 43.0 °C
Full Load
 30.0 hour
@Temperature 32.0 °C
Overcoat End
 32.0 hour
@Temperature 25.0 °C
Light Load
 36.0 hour
@Temperature 25.0 °C
Overcoat End
 36.0 hour
@Temperature 32.0 °C
Full Load
 40.0 hour
@Temperature 10.0 °C
Light Load
 48.0 hour
@Temperature 43.0 °C
Full Chemical
 56.0 hour
@Temperature 10.0 °C
Overcoat End
 60.0 hour
@Temperature 25.0 °C
Full Load
 72.0 hour
@Temperature 10.0 °C
Full Load
 72.0 hour
@Temperature 32.0 °C
Full Chemical
 90.0 hour
@Temperature 25.0 °C
Full Chemical
 120 hour
@Temperature 10.0 °C
Full Chemical
Tack-Free Time 2.00 hour
@Temperature 43.0 °C
 6.00 hour
@Temperature 32.0 °C
 7.00 hour
@Temperature 25.0 °C
 10.0 hour
@Temperature 10.0 °C
 
Descriptive Properties
ColorLight Gray

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chesterton ARC 10 Paste grade machinable composite
3M Scotchkote™ HTX 517 Epoxy HT Lining
3M Scotchkote™ 162PWX Epoxy Coating
3M Scotchkote™ 162HB Epoxy Coating

PPTCHS022 / 138134

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.