MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: An advanced composite formulated to protect concrete and metal surfaces from corrosion and chemical attack. It is normally applied at a thickness of 1-2 mm (40-80 mils) per coat. However, greater single coat film thickness is achievable when spray applied. Non-shrinking, 100% solids. ARC S1HB is a high viscosity, high performance composite lining that is designed to be a spray applied but may also be applied by brush. ARC S1HB allows for uniform coverage over rough surfaces and yields excellent immersion exposures. The cured ARC S1HB provides a barrier film with adhesion and resistance to corrosion.

Benefits:

  • High build capability for coverage over irregular surfaces.
  • Outlasts conventional paints and coatings
  • Long pot life allow for ease of use
  • 100% solids, no shrinkage on cure
  • Outstanding adhesion insures reliable performance
  • Able to be high voltage spark tested for pinhole free films.

Suggested Uses:

  • Bar Screen Chambers
  • Junction/Splitter Boxes
  • collection system Piping
  • Digesters
  • Sewer Piping
  • Waste water Clarifiers
  • Manholes
  • Thickener Tanks
  • ”Other” Concrete and Metal Structures

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
Tensile Strength at Break 38.7 MPa5610 psiASTM D638
Elongation at Break 6.0 %6.0 %ASTM D638
Flexural Strength 57.6 MPa8360 psiASTM D790
Flexural Modulus 2.96 GPa430 ksiASTM D790
Compressive Strength 85.43 MPa12390 psiASTM D695
Adhesive Bond Strength 10.1 MPa1460 psiDry Concrete; ASTM D4541
 >= 13.8 MPa>= 2000 psiMetal; ASTM D4541
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 52.0 °C126 °FWet Service
 80.0 °C176 °FDry Service
 
Processing PropertiesMetricEnglishComments
Cure Time  480 min
@Temperature 43.0 °C
8.00 hour
@Temperature 109 °F
Light Load
 960 min
@Temperature 43.0 °C
16.0 hour
@Temperature 109 °F
Overcoat End
 1080 min
@Temperature 32.0 °C
18.0 hour
@Temperature 89.6 °F
Light Load
 1440 min
@Temperature 43.0 °C
24.0 hour
@Temperature 109 °F
Full Load
 1800 min
@Temperature 32.0 °C
30.0 hour
@Temperature 89.6 °F
Overcoat End
 1920 min
@Temperature 25.0 °C
32.0 hour
@Temperature 77.0 °F
Light Load
 2160 min
@Temperature 25.0 °C
36.0 hour
@Temperature 77.0 °F
Overcoat End
 2160 min
@Temperature 32.0 °C
36.0 hour
@Temperature 89.6 °F
Full Load
 2400 min
@Temperature 10.0 °C
40.0 hour
@Temperature 50.0 °F
Light Load
 2880 min
@Temperature 43.0 °C
48.0 hour
@Temperature 109 °F
Full Chemical
 3360 min
@Temperature 10.0 °C
56.0 hour
@Temperature 50.0 °F
Overcoat End
 3600 min
@Temperature 25.0 °C
60.0 hour
@Temperature 77.0 °F
Full Load
 4320 min
@Temperature 10.0 °C
72.0 hour
@Temperature 50.0 °F
Full Load
 4320 min
@Temperature 32.0 °C
72.0 hour
@Temperature 89.6 °F
Full Chemical
 5400 min
@Temperature 25.0 °C
90.0 hour
@Temperature 77.0 °F
Full Chemical
 7200 min
@Temperature 10.0 °C
120 hour
@Temperature 50.0 °F
Full Chemical
Tack-Free Time  120 min
@Temperature 43.0 °C
2.00 hour
@Temperature 109 °F
 360 min
@Temperature 32.0 °C
6.00 hour
@Temperature 89.6 °F
 420 min
@Temperature 25.0 °C
7.00 hour
@Temperature 77.0 °F
 600 min
@Temperature 10.0 °C
10.0 hour
@Temperature 50.0 °F
 
Descriptive Properties
ColorLight Gray

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chesterton ARC 10 Paste grade machinable composite
3M Scotchkote™ HTX 517 Epoxy HT Lining
3M Scotchkote™ 162PWX Epoxy Coating
3M Scotchkote™ 162HB Epoxy Coating

PPTCHS022 / 138134

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.