MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Kendall® L-427 Super Blu® NLGI Grade 2
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Kendall® L-427 Super Blu is a high-quality, multipurpose, extreme-pressure (EP) lithium complex grease developed for the lubrication of automotive and industrial equipment operating under heavy loads and at moderate to high temperatures. It is NLGI GC-LB certified for use as a multipurpose automotive wheel bearing and chassis lubricant. L-427 Super Blu is manufactured with high-quality paraffinic base oils thickened with lithium complex soap. It is fortified with extreme-pressure and antiwear additives, a tackifier, and rust and oxidation inhibitors to provide excellent wear protection, excellent thermal stability at high temperatures, and excellent resistance to corrosion and water washout. It forms an effective seal to help minimize bearing contamination and provides a high level of adhesion to the bearing surface for improved retention, reduced leakage and enhanced resistance to water washout.

Applications:

  • Wheel bearings of passenger cars, trucks, high-performance vehicles, sport utility vehicles and motorcycles, particularly vehicles with disc brakes
  • Ball joints, universal joints, other chassis parts and water pumps on passenger cars, trucks and other mobile equipment
  • Heavily loaded plain and rolling-element bearings in industrial and mobile equipment
Features/Benefits:
  • Excellent performance over a wide temperature range
  • High load-carrying capacity
  • Excellent wear protection
  • Protects against rust and corrosion
  • Excellent resistance to water washout
  • NLGI GC-LB certified

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.50 lb/gal
Viscosity Measurement 139Index
Saybolt Viscosity at 100°F 801 SUS
Saybolt Viscosity at 210°F 97 SUS
Kinematic Viscosity at 40°C (104°F) 155 cSt
Kinematic Viscosity at 100°C (212°F) 19 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
Pressure Drop; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 250 kgASTM D2596
Four Ball Wear 0.450 mmScar Diameter; ASTM D4172
Penetration P(60), 1/10 mm 265 - 295ASTM D217
Timken Test 45.0 lbASTM D2782
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -40.0 °C
Dropping Point 260 °C
 
Descriptive Properties
ColorBlue
ThickenerLithium Complex
Water Washout Resistance0.05Weight Loss @ 175°F, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kolon H11P(F) Optical film for BLU

WCON5326 / 198579

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.