MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker ELASTOSIL® R 533/60 VPR OH US K540 HCR Silicone
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® R 533/60 VPR OH US K540 is a two component addition curing HCR silicone for the manufacture of silicone-insulated wires and cables. Special features:
  • good mechanical and electrical properties
  • good rheological properties
  • good heat stability
  • in case of fire low smoke density
  • the insulation is free of halogens regardless of the chosen curing method
  • the insulation is free from peroxide split products
Application: Heavy duty cables, where low volatiles, good abrasion resistance, high flexing durability or high mechanical strength are required.

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccDIN EN ISO 1183-1 A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070DIN 53505
Tensile Strength 9.198 MPa1334 psiDIN 53404 S1
Elongation at Break 480 %480 %DIN 53404 S1
Tear Strength 35.1 kN/m200 pliDie B; ASTM D624 B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmDIN IEC 93
Dielectric Constant 2.9
@Frequency 50 Hz
2.9
@Frequency 50 Hz
DIN VDE 0303
Dielectric Strength 23.0 kV/mm584 kV/inDIN IEC 243-2
Dissipation Factor 0.00020
@Frequency 50 Hz
0.00020
@Frequency 50 Hz
DIN VDE 0303
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3842/60 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3071/60 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3005/60 A/B Liquid Silicone Rubber
Wacker ELASTOSIL® R 427/70 High Strength Silicone Base
Wacker Elastosil® R 420/70 Silicone Rubber

PWACK9914 / 197513

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.