MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QM Thixo Agent Thixotropic Additive for Condensation Cure Moldmaking
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: QM Thixo Agent is an additive for Quantum Silicones’ QM 100 moldmaking series. This additive can be used at a 1% level with a QM 100 series base or at a 10% level when used with QM Cat Blue or QM Cat Purple. QM Thixo Agent will cause the material to exhibit non-slump behavior at a thickness of ~ 0.5” without changing the cured properties of the QM 100 series material. This product is ideal for glove molding, lay-up molding, spray applications or any application where a thixotropic moldmaking material is required. The cured rubber has outstanding mechanical properties and good shelf-life stability.

Key Features:

  • Non-slump to ~ 0.5”
  • Fast de-mold time
  • Can vary thixotrophy as needed
For use with QM 113, QM 118, QM 122, QM 128, QM 135 and QM 140

Main Applications:

  • Spray applications
  • Glove molding

    Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccUncatalyzed, QM Thixo Agent
Viscosity 2000 cPUncatalyzed, QM Thixo Agent
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 6.00 hourDemold time, Catalyzed, QM Cat Purple with 10% Thixo Agent
 4.00 - 6.00 hourDemold time, Catalyzed, QM Cat Blue with 10% Thixo Agent
Tack-Free Time 45.0 - 90.0 minCatalyzed, QM Cat Purple with 10% Thixo Agent
 90.0 - 180 minCatalyzed, QM Cat Blue with 10% Thixo Agent
Pot Life 15.0 minCatalyzed, QM Cat Purple with 10% Thixo Agent
 20.0 minCatalyzed, QM Cat Blue with 10% Thixo Agent
 
Descriptive Properties
AppearanceViscous LiquidUncatalyzed, QM Thixo Agent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Corporation Bisco™ HT-820 Cellular Silicone Foam
Rogers Arlon 44426R010 0.010" Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate
Overview of materials for Silicone Rubber
Momentive Performance Materials SS4171P Addition Cure Silicone Rubber Molding Compounds
Momentive Performance Materials Silopren™ LSR 4040 Liquid Silicone Rubber - Healthcare

PACC2074 / 199462

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.