Applications- High pressure die casting
- Gravity die casting
- Sand casting
Advantages - Light weight
- No pre-heating required
- Low thermal heat sink
- Excellent mechanical properties
- Excellent resistance to erosion
- Excellent scull release
- Non-wetted by molten aluminum
- No iron contamination
- Low maintenance
- Reduced holding temperatures
Information provided by Pyrotek. |