MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 2.1 & (c) 2.2.

Applications:

  • Medium duty shrink film
  • Shopper bags
  • Form fill and seal packaging

Additives: Barefoot

Advantages: Good mechanical properties and stiffness

Information provided by Titan Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Base Resin Density 0.922 g/ccASTM D1505
Thickness 50.0 micronsextruded at 2.5:1 BUR
Base Resin Melt Index 0.75 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 370 %ASTM D882
Film Elongation at Break, TD 560 %ASTM D882
Elmendorf Tear Strength, MD 7.00 g/micronASTM D1922
Elmendorf Tear Strength, TD 4.00 g/micronASTM D1922
Dart Drop 4.00 g/micronASTM D1709
Film Tensile Strength at Break, MD 27.5 MPaASTM D882
Film Tensile Strength at Break, TD 24.5 MPaASTM D882
1% Secant Modulus, MD 31291 psiASTM D882
1% Secant Modulus, TD 34136 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 93.0 °Cresin; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 160 - 190 °C
Blow-up Ratio (BUR) 1.5 - 3.0
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Chemical Titan TITANLENE® LDF265YZ Low density polyethylene
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips 4538B LDPE Injection Molding Resin
Chevron Phillips KN 230B LDPE Injection Molding Resin
LG Chemical LUTENE FB0300 LDPE Blown Film Grade

PTITAN63 / 70429

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.