MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zeus Polyimide Coating
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Unfilled

Material Notes: Zeus polyimide tubing can be produced in extremely small dimensions, yet it retains strength and pushability whether for vascular catheters or non-medical deployments. Polyimide can also be provided as a coating for over-the-wire (OTW; PI insulated wire) applications. Polyimide coating for electrical leads provides insulation in addition to a low-friction surface for easier positioning or placement. Polyimide can also be provided in a layered composite-type construction to further tailor tubing or coating properties.

Specific applications include catheters (vascular, structural heart, electrophysiology, urinary), lumen for guidewires, lead wire delivery devices, stone retrieval devices, and vascular closure devices.

Available in tubing (pull wires, lead (insulated) wire, guidewires, coated wire) and composite/multi-layer construction.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.44 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 239 MPaASTM D638
Elongation at Break 105 %ASTM D638
Coefficient of Friction 0.49ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 7757 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 220 °C
Decomposition Temperature 504 °Cin air
Flammability, UL94 V-0
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Radiation Resistance Very Good

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZEUS980 / 280558

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.