Description: Tensile strength, Elongation, Oil resistance, Abrasion resistance, Softness, Whiteness Application: Nitrile Glove (Examination Glove, Clean Room Glove), Supported Glove (Industrial Glove) CSA No. 9010-81-5 and 7732-18-5 Information provided by LG Chemical |