MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil 27 Mobil Mist Lube Series
Categories: Fluid; Lubricant

Material Notes: Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from high quality, solvent refined base stocks and a unique additive system designed for optimum reclassifying properties. They have a high resistance to oxidation and good extreme pressure and anti-wear properties. The products have enhanced surface wetting capabilities and they reclassify (or agglomerate) readily from a mist to a liquid when the mist is subjected to extreme turbulence or is impinged onto a surface at high velocity. This allows a lubricating film to form on bearings and gears and prevents stray mist from escaping through narrow apertures into the atmosphere. The four viscosity grades in the Mobil Mist Lube Series, ranging from ISO VG 32 to 460, allow the machine designer to choose the product most suitable for proper mist lubrication of machine elements. The heavier grades are used on ways, gears, and slow-speed, heavily loaded bearings, while the lower viscosity grades are used in high-speed bearings.

Mobil Mist Lube Series oils are designed for use in all oil mist lubrication systems. Such systems work by dispersing very small droplets of oil in smoothly flowing air, distributing the oil mist to the points of application and mechanically condensing the mist, causing the oil to impinge on and wet the surfaces to be lubricated. The higher viscosity Mobil Mist Lube grades may require thermal misting devices to form proper dispersions when ambient temperatures are moderate or low. Mobil Mist Lube 24 is suitable for oil / air delivery systems such as airline oilers. Specific applications include: Industrial gearing such as cooling tower gearboxes; Slow-speed, heavily-loaded bearings (higher viscosity grades); High-speed bearings (lower viscosity grades); Machine tools, ways and screws; Process pumps, electric motors and blowers; Steam turbines and electric motors

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc
@Temperature 15.6 °C
0.0322 lb/in³
@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 9595Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 100 cSt100 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 11.2 cSt11.2 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Load Wear Index 4848ASTM D2783
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)ASTM D2783
Four Ball Wear 0.300 mm0.0118 in20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172
Timken Test 29500 g65.0 lb
 
Thermal PropertiesMetricEnglishComments
Pour Point -12.0 °C10.4 °FASTM D97
Flash Point 234 °C453 °FASTM D92
 
Descriptive Properties
FZG Scuffing, DIN 5182, A/8.3/90, Fail Stage12+
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil 24 Mobil DTE 20 Series
ExxonMobil 26 Mobil DTE 20 Series

WEXXON238 / 75663

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.