MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Momentive Performance Materials GE Silicones Enduris 3400 Silicone Roof Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: GE Enduris 3400 silicone roof coating is a liquid applied one-part silicone coating that is an excellent candidate to consider for use in roofing applications as the weathering coat over a variety of roofing materials including spray applied polyurethane foam, water-borne coatings (acrylic), PVC membranes, and galvanized/coated metals. Enduris 3400 silicone roof coating forms a durable, breathable, watertight and weatherproof barrier that is extremely resistant to degradation from natural weathering.

Features: Lowers Energy Costs, Seamless, Monolithic Air Barrier, Simple Installation.

Applications: Silicone Durability, Versatile Application, Ease of Use, Ample Work Life, Accelerated Cure Rate, Low Temperature Storage.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/inĀ³WPSTM P-14
Solids Content 85 %85 %By weight.; WPSTM P-19
Volatile Organic Compounds (VOC) Content <= 228 g/l<= 228 g/lEPA Method 24
Viscosity 4360 cP4360 cPWPSTM C-560
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 34 - 4034 - 40ASTM D2240
Tensile Strength 1.31 MPa190 psiASTM D412
Elongation at Break 213 %213 %ASTM D412
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.910.91SCM3402 (white).; ASTM C1371
Reflection Coefficient, Visible (0-1) 0.820.82Solar Reflectance; ASTM C1549
 
Processing PropertiesMetricEnglishComments
Tack-Free Time 45.0 min0.750 hourWPSTM E-86
 
Descriptive Properties
ColorWhite, medium gray, tan, dark gray.
Skin Over Time30-40 minutesWPSTM C-560
SRI Value90ASTM E1980. Enduris 3502 (white).

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9910 / 265719

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.