MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil 824 Mobil SHC 800 Series
Categories: Fluid; Lubricant

Material Notes: Mobil SHC 800 Series turbine oils are designed specifically to meet the needs of the most severe industrial gas turbine applications with a nominal 10,000 hour TOST life. They are recommended for the lubrication of land-based gas turbines, particularly units under 3,000 hp used as standby power units, and in some types of total energy and combined cycle (gas/steam) systems. This innovative product family is formulated from wax-free synthesized hydrocarbons and a unique additive system. This formula provides outstanding low temperature fluiditiy and exceptional resistance to degradation at high temperatures well beyond the capabilities of premium quality mineral oils. Mobil SHC 800 Series lubricants also provide excellent antiwear properties as well as protection against rust and corrosion plus good air release performance and resistance to foaming. These characteristics provide superior resistance to thermal/oxidative degradation during the heat soaking period after shutdown and permit rapid oil circulation at low temperatures during start-up. Degradation resistance is a key attribute in avoiding harmful deposits that can interfere with lubrication supply to the bearings or foul critical servo-valves. This is a particular issue when gas turbines are running in cycling mode and experience multiple thermal stress cycles. Since low temperature fluidity and high viscosity index are inherent characteristics of the fluids, they do not change in service as a result of mechanical shearing or repeated cycling from low to high temperatures. Mobil SHC 800 Series oils are fully compatible with mineral oils, but admixture will detract from its superior performance properties. These progressive products, which have been proven in very severe gas turbine service over many years, are preferred by users because of their outstanding stability and equipment protection under the most severe, high temperature conditions, and because of their easy start-up at low ambient temperature. This performance results in excellent equipment reliability and minimized downtime.

Mobil SHC 800 Series turbine oils are designed specifically to meet the needs of the most severe industrial gas turbine applications and ancillary equipment. Specific applications include: Severe stationary gas turbine applications, particularly units under 3,000hp, for stand-by power generation; Industrial gas turbines operating in low ambient and remote areas; Total energy systems

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.830 g/cc
@Temperature 15.0 °C
0.830 g/cc
@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 135135Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 31.5 cSt31.5 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 5.9 cSt5.9 cStASTM D445
Oxidative Stability 9500 hour9500 hourTurbine Oil Stability Test (TOST); ASTM D943
 
Thermal PropertiesMetricEnglishComments
Pour Point <= -54.0 °C<= -65.2 °FASTM D97
Flash Point 248 °C478 °FASTM D92
 
Descriptive Properties
Air Release, ASTM D3427, minutes1@ 50°C
Foam Sequence I, ASTM D96810/0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Mobil Vactra 1
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel
Assab Steels QRO 90 SUPREME Hot Work Steel
Assab Steels HOTVAR Hot Work Steel
AISI Type H13 Hot Work Tool Steel

WEXXON148 / 75573

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.