  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Elastosil® R plus 4846/30 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: HTV silicone rubbers of the grade ELASTOSIL® R plus 4846/30 are oil-bleeding one-component PT-curing compounds for the manufacture of molded articles. The vulcanizates are opaque and form a thin oil film with lubricating properties shortly after the curing process. As the crosslinking system is based on platinum cure no peroxide decomposition products can be formed during curing.

Application: The grade is suitable for the manufacture of molded articles for technical applications. Specially thick walled articles can take advantage of the fast curing material.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030DIN 53505
Tensile Strength at Break 10.0 MPa1450 psiDIN 53504 S1
Elongation at Break 1000 %1000 %DIN 53504 S1
Tear Strength 32.0 kN/m183 pliASTM D624 B
Compression Set  19 %
@Temperature 175 °C,
Time 79200 sec
19 %
@Temperature 347 °F,
Time 22.0 hour
post cured 4h/200°C; DIN ISO 815-B
 40 %
@Temperature 175 °C,
Time 79200 sec
40 %
@Temperature 347 °F,
Time 22.0 hour
DIN ISO 815-B
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
0.250 hour
@Treatment Temp. 329 °F
post cured 4h/200°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9301 / 204830

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.