MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
OCTAL DPET™ PET Sheet
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Clear rigid sheet for use in general packaging; foam, fill, and seal; dairy products; and lamination. DPET™ sheet is produced directly from PET melt resin, resulting in enhanced optical and mechanical properties.

Information provided by OCTAL Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccASTM D1503
Thickness 200 - 1200 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 564 - 634 kg(f)/cm²ASTM D882
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 90 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 121 - 154 °CThermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kostat ICP-STAT ICD-1001 PET Sheet
Pearl Engineering PEPLPET B-101C PET Sheet Grade
GEHR Plastics PET Polyethylene Terephthalate
Manifattura Cattaneo PET Polyethylene Terephthalate
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced

POCTAL990 / 133504

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.