MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Buckeye Polymers BP RPP 4012 TU Polypropylene, 40% Mineral Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Talc Filler

Material Notes: UV Stabilized

This Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resistance to some aggressive chemical agents.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inASTM D955
Melt Flow 12 g/10 min12 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 29.6 MPa4290 psiASTM D638
Flexural Modulus 3.20 GPa464 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C241 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene
Aclo Accutech Polypropylene CP0437T40V Copolymer Talc Reinforced
Adell RA-18 Copolymer Polypropylene, 40% Talc Filled
A. Schulman ComAlloy Aqualoy® 125 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL
A. Schulman Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled

PBUK05 / 27860

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.