MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Achieve™ Advanced PP3854 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Achieve™ Advanced PP3854 is a homopolymer resin produced using ExxonMobil  Exxpol™ Technology designed for spun bound technology. Narrow molecular weight distribution of the resin allows for excellent uniformity, finer fibers and high tensile strength allowing for creative innovations in applications and possible down gauging.  

Availability:  Latin America, North America.  Features:  clean/high purity, low smoke emission.   Applications: personal care , spun bond nonwovens, textile applications.  Appearance:  Natural Color.  Forms:  pellets.  Processing Method: fiber (spinning) extrusion, filament extrusion.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ExxonMobil Method
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 230 °C
24 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graft Polymer GRAFTABOND™ PPH-MAH 20025 CA Maleic anhydride functioned Homopolymer Polypropylene
Graft Polymer GRAFTABOND™ PPH-MAH 15025 CA Maleic anhydride functioned Homopolymer Polypropylene
ExxonMobil Achieve™ Advanced PP6936G2 Polypropylene Homopolymer
ExxonMobil Achieve™ 6936G2 Polypropylene Homopolymer
Esenttia 35H35 Homopolymer Polypropylene

PEX98969 / 238350

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.