MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röhm ACRYLITE® Film White WF007 PMMA
Categories: Polymer; Film; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: PLEXIGLAS® Film WF007 is a high weather resistant and glossy white acrylic film for destructible labels and tapes. The film is 100% acrylic based and therefore it contains no plasticizer and it is a completely PVC free polymer. Thanks to its proprietary acrylic polymer formulation, the film displays a defined low elongation at break and high crack propagation. Due to its excellent performance under long term weathering and UV light exposure, PLEXIGLAS® Film WF007 does not present color change or yellowing. Its glossy and very smooth surface leads the film to have an excellent graphic quality surface.

Application: PLEXIGLAS® Film WF007 is used as a single face layer in high UV and weathering resistant destructible labels and tapes.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³DIN 53479
Surface Tension 50 dynes/cm50 dynes/cmDIN 53364
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 41.0 MPa5950 psiISO 527-3
Elongation at Break 24.6 %24.6 %ISO 527-3
Elongation at Yield 5.7 %5.7 %ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 101 °C214 °FISO 11357
 
Optical PropertiesMetricEnglishComments
UV Transmittance 0.00 %
@Wavelength 280 - 380 nm
0.00 %
@Wavelength 280 - 380 nm
DIN EN 410

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm PLEXIGLAS® GS Clear 2458 3 mm UV transmitting PMMA
Röhm PLEXIGLAS® Film blue 5F005 PMMA
Röhm DEGALAN® VP 1017 F Acrylic Resin
Röhm Acrylite® S10/8H Compound Molding and Extrusion
Röhm ACRYLITE® LED LD24 Acrylic Polymer

PEVONIL049 / 196253

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.