MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems Accura® 25 Plastic for SLA® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: For use with solid-state stereolithography (SLA®) systems.

    Applications
  • Functional components for assemblies and mock-ups for:
    • Automotive styling parts — trim, fascia, and other components
    • Consumer electronic components
    • Toys
    • Snap fit assemblies
  • Master patterns for RTV/silicone molding
  • Replace CNC machining of polypropylene to produce short-run plastic parts
  • Simulate injection molded parts
  • Concept and marketing models

    Features
  • Look and feel of molded polypropylene
  • High flexibility with excellent shape retention
  • Outstanding feature resolution and accuracy
  • High production speed
  • Fully developed and tested build styles

All information provided by 3D Systems.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. North American leaders in providing high quality Rapid Prototyping and Additive Manufacturing solutions using all major 3D printing systems including SLA technology. Free 3D printing quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
@Temperature 25.0 °C
Liquid
 1.19 g/cc
@Temperature 25.0 °C
Solid
Viscosity 250 cP
@Temperature 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80
Tensile Strength 55.0 - 58.0 MPaASTM D638
Elongation at Break 13 - 20 %ASTM D638
Tensile Modulus 1590 - 1660 MPaASTM D638
Flexural Strength 55.0 - 58.0 MPaASTM D790
Flexural Modulus 1380 - 1660 MPa
Izod Impact, Notched 19.0 - 24.0 J/mASTM D256
Penetration 4.2mils
 
Thermal PropertiesOriginal ValueComments
CTE, linear 107 µm/m-°C
@Temperature 0.000 - 20.0 °C
T
 151 µm/m-°C
@Temperature 90.0 - 150 °C
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 58.0 - 63.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 55.0 °CASTM D648
Glass Transition Temp, Tg 72.0 - 74.0 °CDMA, E"
 
Descriptive Properties
AppearanceWhite
Critical Exposure (mJ/cm²)10.5
Tested Build StylesFAST™, EXACT™, Exact HR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® RIGUR RGD450 Simulated Polypropylene 3D Printing Polymer
Overview of materials for PVC, Molded
3D Systems Accura® 10 Plastic for SLA® Systems
Overview of materials for Acetal Copolymer, Unreinforced
Stratasys® RGD8425-DM Rigid Opaque Digital Material

PAPPR103 / 83482

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.