MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta RSGFR4 Sheet Ground Rod
Categories: Polymer; Thermoset

Material Notes: RSGFR4 is a sheet ground rod produced from sheets of material that conform to NEMA FR-4, ANSI/NEMA FR-4 and MIL-I-24768/27 Type GEE-F. None of these specifications have any requirements for sheet ground rod.

Information provided by Norplex Micarta.

Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 105
Tensile Strength 42500 psiCondition A
Tensile Modulus 3200 ksi
Flexural Strength 67500 psiCondition A
Flexural Modulus 2500 ksi
Compressive Strength 47500 psiCondition A
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 120 °C
UL RTI, Mechanical with Impact 130 °C
Flammability, UL94 HBCondition A
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.0300 %Condition D; ASTM D-349
 
Descriptive Properties
Rod Diameter0.5 inch (1.3 mm)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNORPM918 / 323355

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.