MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Nicusil™ Mac-Nicusil™ 3-WM Braze Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: High-purity silver/copper/nickel alloy for vacuum brazing.

Applications:

  • Aero-engines (OEM and repair)
  • Aerospace fuel-line assemblies
  • Vacuum tubes
  • Wave guide and Klystron assemblies
  • Power supply surge arrestors
  • Automotive components

information provided by Morgan Advanced Materials

Key Words: Braze Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.99 g/cc0.361 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 330 MPa47900 psi
Elongation at Break 32 %32 %2 in/50mm gage section
Compressive Yield Strength 207 MPa30000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000340 ohm-cm0.00000340 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 223 W/m-K1550 BTU-in/hr-ft²-°Fcalculated
Melting Point 780 - 795 °C1440 - 1460 °F
Solidus 780 °C1440 °F
Liquidus 795 °C1460 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 815 - 840 °C1500 - 1540 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd <= 0.0010 %<= 0.0010 %
Carbon, C <= 0.010 %<= 0.010 %
Copper, Cu 28.1 %28.1 %nominal
Lead, Pb <= 0.0020 %<= 0.0020 %
Nickel, Ni 0.75 %0.75 %nominal
Phosphorus, P <= 0.0020 %<= 0.0020 %
Silver, Ag 71.15 %71.15 %nominal
Zinc, Zn <= 0.0010 %<= 0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Nicoro™ Mac-Nicoro™-WM Braze Alloy
Morgan Advanced Ceramics Palcusil™ Mac-Palcusil™10-WM Braze Alloy
Morgan Advanced Ceramics 50Ni-50Cu Mac-50Ni/50Cu-WM Braze Alloy
Morgan Advanced Ceramics Palnicro™ Mac-Palnicro™ 30-WM Braze Alloy
Morgan Advanced Ceramics Cusil™ Mac-Cusil™-WM Braze Alloy

CMORF8018 / 203495

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.