MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 216E01 Non-Sag Dam Applications Adhesive
Categories: Polymer; Adhesive; Thermoset; Filled/Reinforced Thermoset

Material Notes: TRA-BOND 216E01 is a thixotropic, two-part adhesive formulated specifically for applications where a high-fill, non-sag adhesive is required. TRA-BOND 216E01 works in concert with TRA-BOND 216E02 to perform `dam` and `fill` functions. It bonds exceptionally well to ceramic, metal, glass, plastic and other substrates. Fully cured TRA-BOND 216E01 provides excellent resistance to water, gases and vapors, petroleum products, salt solutions, acids and other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.080 %0.080 %
Viscosity 124000 cP
@Temperature 25.0 °C
124000 cP
@Temperature 77.0 °F
Mixed (rv #7, 10 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Adhesive Bond Strength 21.4 MPa3100 psiLap shear, alum to alum, 4 hrs @ 65°C
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 65.0 °C149 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 4320 min
@Temperature 25.0 °C
72.0 hour
@Temperature 77.0 °F
Pot Life 180 min180 min40 grams
Working Life 480 min480 min40 grams
 
Descriptive Properties
Color Black
Mix Ratio, parts by weight100/57Resin/Hardener
Thixotropic Index 5.51 rpm/10 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC048 / 70976

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.