MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro Desmodur® ME-230 + BaytecT20 + Baytec XL B, 74A Polyurethane, MDI-Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characteristics:
Properties:
  • Good abrasion resistance
  • Excellent hydrolysis resistance
  • Low temperature performance
  • High resilience
  • Good microbial resistance
Comments:
  • Suitable for skate board and roller skate wheels
  • Production of seals, gaskets & hydrocyclones
  • Ideal for snow plow blades

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccDesmodur ME-230
Viscosity 8.0 cPBaytec XL B
 80 cPDesmodur ME-230
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74ASTM D2240
Tensile Strength at Break 21.2 MPaASTM D412
Elongation at Break 530 %ASTM D412
100% Modulus 0.00283 GPa
@Strain 100 %
ASTM D412
200% Modulus 0.00400 GPa
@Strain 200 %
ASTM D412
300% Modulus 0.00570 GPa
@Strain 300 %
ASTM D412
Resilience 68[%], Bayshore; ASTM D2632
Tear Strength 110 pliSplit; ASTM D1938
 380 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 14
@Load 1.00 kg
H-18 wheel; ASTM D4060
Compression Set 19 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395-B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 45.0 - 60.0 °CBaytec XL B
 65.0 °CDesmodur ME-230
 70.0 °CBaytec T20
Mold Temperature 80.0 °C
Pot Life 6.00 - 7.00 min
 
Descriptive Properties
AppearanceliquidDesmodur ME-230
 solidBaytec T20
 solidBaytec XL B
Content0.025Parts by weight of Dabco T-12 per 100 parts of Baytec XL B
 0.5-0.7Parts by weight of Dabco 33LV per 100 parts of Baytec XL B
 100Parts by weight of Desmodur ME-230 prepolymer
 1000 EWNCO, Baytec T20
 12.5Parts by weight of Baytec XL B
 22.7-23.3%NCO, Desmodur ME-230
 237.5Parts by weight of Baytec T20
 45 EWNCO, Baytec XL B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow SZ-1175 Silicone Surfactant
Lanxess Addocat® 104 PU Catalyst/Activator
Covestro Desmodur® MS-090 + Baytec XL B/Baytec XL HQEE, 93A/47D Polyurethane, MDI- Ester
Covestro Desmodur® ME-230 + BaytecT20 + Baytec XL B, 97A/55D Polyurethane, MDI-Ester
Covestro Desmodur® ME-230 + BaytecT20 + Baytec XL B, 85A Polyurethane, MDI-Ester

PCOVEST0483 / 202266

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.