MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil 10W-30 Exxon XD-3
Categories: Fluid; Lubricant

Material Notes: Exxon XD-3 10W-30 and 15W-40 are premium diesel engine oils formulated to provide excellent protection to modern, high performance diesel engines used in severe on and off-highway applications. These multigrade diesel engine oils are designed using top quality, highly refined base oils and an effective additive system that protects all parts of the engine. Exxon XD-3 is recommended for use in a wide range of heavy-duty applications and operating environments and meets the latest API specifications for gasoline engines used in mixed fleets.

Naturally aspirated and turbo-charged equipment powered equipment manufactured; Over the road heavy and light duty diesel trucks; Pickup trucks and sport utility vehicles with diesel or gasoline engines; Off-Highway operations including: construction, mining, quarrying, and agriculture

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.866 g/cc
@Temperature 15.0 °C
0.0313 lb/in³
@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 145145Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 74 cSt74 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 11.5 cSt11.5 cStASTM D445
Ash 1.1 %1.1 %Sulfated Ash, wt%; ASTM D874
 
Chemical PropertiesMetricEnglishComments
Total Base Number 1010mg KOH/g; ASTM D2896
 
Thermal PropertiesMetricEnglishComments
Pour Point -33.0 °C-27.4 °FASTM D97
Flash Point 240 °C464 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON008 / 75433

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.