MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ruthenium, Ru; Annealed
Categories: Metal; Nonferrous Metal; Precious Metal; Pure Element

Material Notes: Annealed applies only to tensile and/or hardness values; other property values are typical of the element.

Physical Form: Silver-White Metal; Hexagonal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 12.3 g/cc0.444 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 101.07101.071995
Atomic Number 4444
Thermal Neutron Cross Section 2.6 barns/atom2.6 barns/atom
X-ray Absorption Edge 0.56 Å0.56 ÅK
 3.84133 Å3.84133 ÅLI
 4.17654 Å4.17654 ÅLII
 4.36632 Å4.36632 ÅLIII
Electrode Potential 0.45 V0.45 V
Electronegativity 2.22.2Pauling
Ionic Radius 0.670 Å0.670 ÅCrystal Ionic Radius for Valence +4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 220220Converted from Vickers for 3000 kg load/10 mm ball Brinell test. Annealed
Hardness, Rockwell A 6060Converted from Vickers. Annealed
Hardness, Rockwell B 9696Converted from Vickers. Annealed
Hardness, Rockwell C 1818Converted from Vickers. Annealed
Hardness, Vickers 220220Annealed
Tensile Strength, Ultimate 370 MPa53700 psiAnnealed
Modulus of Elasticity 414 GPa60000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000720 ohm-cm0.00000720 ohm-cm
Magnetic Susceptibility 5.6e-75.6e-7cgs/g
Critical Magnetic Field Strength, Oersted 67 - 7167 - 71
Critical Superconducting Temperature 0.475 - 0.505 K0.475 - 0.505 K
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 193 J/g83.0 BTU/lb
Heat of Vaporization 6196 J/g2666 BTU/lb
CTE, linear 9.60 µm/m-°C
@Temperature 20.0 - 100 °C
5.33 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.2127 J/g-°C0.05084 BTU/lb-°FGas
 0.243 J/g-°C0.0581 BTU/lb-°F
Thermal Conductivity 116 W/m-K805 BTU-in/hr-ft²-°F
Melting Point 2310 °C4190 °F
Boiling Point 4150 °C7500 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molCrystal
 642.7 kJ/mol642.7 kJ/molGas
 
Optical PropertiesMetricEnglishComments
Reflection Coefficient, Visible (0-1) 0.630.63
 
Component Elements PropertiesMetricEnglishComments
Ruthenium, Ru 100 %100 %
 
Descriptive Properties
CAS Number7440-18-8
SolubilityInorganic in Acid and Aqua Regia

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rhodium, Rh; Annealed
Ruthenium, Ru; Hot Rolled Bar
Molybdenum, Mo, Annealed
Silver, Ag
Aluminum, Al

AMERu00 / 97

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.