Bonding: PP, PE Typical Applications: Flippers; Gas mask; Industrial parts; Toothbrush & Shaver Material Advantages: Excellent adhesion to PP, PE; Good UV stability; Good weather resistance; Excellent mechanical properties Information provided by Everlon TPE/TPR Manufacturing Experts |