MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Regalite™ C6100 Hydrocarbon Resin
Categories: Other Engineering Material

Material Notes: Product Description: Regalite™ C6100 hydrocarbon resin is a very light color, partially hydrogenated, modified aliphatic resin designed as an excellent tackifier for the midblock of thermoplastic block copolymers, including styrene-isoprene-styrene (SIS), [low, medium, and high styrene content] styrene ethylene butylene styrene (SEBS) and styrene-butadiene-styrene (SBS). It also shows excellent compatibility with ethylene vinyl acetate (EVA). Regalite™ C6100 is recommended for use in a variety of hot melt adhesives, including nonwoven assembly, packaging, bookbinding, glue sticks, and pressure-sensitive tape and label adhesives.

Application/Uses:

  • Automotive
  • Building and Construction
  • Hot Melt Adhesives
  • Nonwovens
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Wax Modification

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Viscosity 130 cP
@Temperature 190 °C
Melt
 750 cP
@Temperature 160 °C
Melt
 5000 cP
@Temperature 140 °C
Melt
Molecular Weight 610 g/molMn
 1010 g/molMw. Mw/Mn ratio = 1.66
 1880 g/molMz
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 43.2 °COnset
 49.4 °CMiddle
 55.7 °CEnd
Ring & Ball Softening Point 100 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Yellow Index 4.5 %ASTM E313
 14.6 %
@Temperature 177 °C,
Time 18000 sec
ASTM E313
 67.4 %
@Temperature 177 °C,
Time 86400 sec
ASTM E313
Gardner Color Number <= 1.0ASTM D6166
 <= 1.02 cm cell; ASTM D6166
 1.9
@Temperature 177 °C,
Time 18000 sec
ASTM D6166
 6.3
@Temperature 177 °C,
Time 86400 sec
ASTM D6166
 
Descriptive Properties
Cloud Point<-50°COMS
 31°CDACP
 60°CMMAP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5542 / 222736

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.