MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis Visico™/ Ambicat™ ME4425 /LE4479 Polyethylene, Silane Crosslinkable Insulation Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Visico " ME4425 / Ambicat " LE4479 is a silane crosslinkable natural compound system designed for insulation of low voltage energy cables. Visico ME4425 is a medium density polyethylene, copolymerized with vinyl silane. Ambicat LE4479 is an ambient crosslinking catalyst masterbatch specially designed to be used with Visico base resins to give reduced radial shrinkage in cables. The system is highly active and crosslinks quickly at ambient conditions, in sauna or in hot water. Cable insulation with a proper mixture of Visico ME4425 (95 parts) and Ambicat LE4479 (5 parts) exhibits excellent thermo-oxidative stability. The combination is suitable for both copper and aluminum conductors. If the insulation is designed to meet the thermo-oxidative ageing demand required by IEC 60502 at 150°C in contact with copper, the addition of 9 parts Ambicat LE4479 to Visico ME4425 is recommended.

Applications: Visico"ME4425 / Ambicat"LE4479 is intended for following applications: Insulation of low voltage energy cables, range up to 6 kV

Specifications: Visico"ME4425 / Ambicat"LE4479 is expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures. ASTM D1248 Type II, Class A, Category 4; HD 604 S1; IEC 60502-1; EN 50290-2-2; HD 603 S1

Typical characteristics: Visico"ME4425 / Ambicat"LE4479 can be described with following typical characteristics:

  • Excellent processing properties
  • Very good curing speed
  • Low scorch allowing long runs and more frequent tooling changes
  • Excellent surface finish
  • Environmentally friendly (free from heavy metals)
  • Reduced radial shrinkage
  • Less smell; more consistent quality (no volatiles)
  • Excellent storage stability
  • No drying prior to extrusion
The addition of metal soaps and basic (high pH) components, like some fillers, stearates and UV-stabilizers, will deactivate the catalyst and is not suitable together with Ambicat. To prevent deactivation of the catalyst during coloring, Ambicat compatible color masterbatches are needed. Please contact your Borealis representatives for additional information.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ISO 1183-1
Melt Flow 1.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.00 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Storage Temperature 10.0 - 30.0 °C50.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 20.0 MPa>= 2900 psi250 mm/min; IEC 60811-501
 >= 14.0 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
>= 2030 psi
@Treatment Temp. 302 °F,
Time 168 hour
After ageing with Cu-conductor; IEC 60811-401
 >= 15.0 MPa
@Treatment Temp. 135 °C,
Time 605000 sec
>= 2180 psi
@Treatment Temp. 275 °F,
Time 168 hour
After ageing; IEC 60811-401
Elongation at Break 0.000 %0.000 %Hot set test - Permanent deformation (200 °C, 0.20 MPa); IEC 60811-507
 60.0 %60.0 %Hot set test - Elongation under load (200 °C, 0.20 MPa); IEC 60811-507
 >= 300 %>= 300 %250 mm/min; IEC 60811-501
 >= 375 %
@Treatment Temp. 135 °C,
Time 605000 sec
>= 375 %
@Treatment Temp. 275 °F,
Time 168 hour
After ageing; IEC 60811-401
 >= 390 %
@Treatment Temp. 150 °C,
Time 605000 sec
>= 390 %
@Treatment Temp. 302 °F,
Time 168 hour
After ageing with Cu-conductor; IEC 60811-401
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.30
@Frequency 50 Hz
2.30
@Frequency 50 Hz
IEC 62631-2-1
 
Processing PropertiesMetricEnglishComments
Zone 1 150 °C302 °F
Zone 2 185 °C365 °F
Zone 3 185 °C365 °F
Zone 4 185 °C365 °F
Die Temperature 185 °C365 °F
Melt Temperature 190 - 195 °C374 - 383 °F
Shelf Life 18.0 Month18.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9931 / 323288

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.