System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
ExxonMobil PPU0009F Polypropylene Impact Copolymer
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Impact Modified; Molded/Extruded
Material Notes:
Product Description: An unstabilized impact copolymer resin designed for automotive and compounding applications.
Availability: Europe
Processing Method: Compounding
Information provided by ExxonMobil
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.900
g/cc
ISO 1183
Melt Flow
14
g/10 min
ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Modulus
160000
psi
ISO527-2
Charpy Impact, Notched
1.40
ft-lb/in²
@Temperature -20.0 °C
ISO 179/1eA
1.90
ft-lb/in²
@Temperature 0.000 °C
ISO 179/1eA
3.80
ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
122
°F
ISO 75-2/A
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
ExxonMobil PP7011L1 Polypropylene Impact Copolymer
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHM-200 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHX-006 Polypropylene Impact Copolymer
ExxonMobil PP4031E2 Polypropylene Impact Copolymer
PEX99433 / 175669
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.