MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SCG Chemicals C6950XXX PVC Wire & Cable Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: C6950XXX is PVC compound product with any color for using in wire and cable application product. The formulation is designed for Flame retardant and low smoke low halogen of Power cable which give good process ability by extrusion.

Applications: Flame retardant cable.

Features: Low smoke, low halogen. Good process ability.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.62 - 1.68 g/cc1.62 - 1.68 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78 - 80
@Time 10.0 sec
78 - 80
@Time 0.00278 hour
ASTM D2240
Tensile Strength 15.0 - 17.0 MPa2180 - 2470 psiIEC 60811-1-1
Elongation at Break 225 - 410 %225 - 410 %IEC 60811-1-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.90e+14 - 5.20e+14 ohm-cm1.90e+14 - 5.20e+14 ohm-cmJIS K6723
 
Thermal PropertiesMetricEnglishComments
Smoke Density 146 - 203146 - 203Nonflaming mode. DMC; ASTM E662
Oxygen Index 40 - 43 %40 - 43 %ASTM D2863
 
Descriptive Properties
AppearancePellet
HCL Emission: PH (%)2.6-3.4TPC Method. Acid Gas Emission: PH
Heat Stability540-640 minTPC Method @ 180°C
Loss of Mass0.2-.06 mg/cm2IEC 60811-3-2. Aging @ 100°C x 168 hrs.
Retention of Elongation at Break (%)74-99IEC 60811-1-2. Aging @ 100°C x 168 hrs.
Retention of Tensile Strength (%)93-108IEC 60811-1-1. Aging @ 100°C x 168 hrs.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC816 / 278073

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.