MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis WG365C Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: WG365C is filled polypropylene compound especially developed for seal-peel purposes. It contains finely dispersed inorganic filler. It can be used as such for cohesive peel-seals or as a blending component. Cas No. 9002-88-4, 9003-07-0

Applications: WG365C is a grade suitable for extrusion coating or in cast film processes.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.62 g/cc0.0585 lb/in³ISO 1183
Filler Content 40.0 %40.0 %ISO 3451
Melt Flow 10.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 50.0 °C<= 122 °F
 
Processing PropertiesMetricEnglishComments
Feed Temperature 300 °C572 °F
Zone 1 200 °C392 °FExtruder
Zone 2 240 °C464 °FExtruder
Zone 3 290 °C554 °FExtruder
Zone 4 300 °C572 °FExtruder
Zone 5 300 °C572 °FExtruder
Adapter Temperature 285 °C545 °F
Die Temperature 300 °C572 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9935 / 323292

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.