MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Syncon® Extra Long Life Grease NLGI No. 00
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant; Polyalphaolefin (PAO)

Material Notes: Description: Conoco Syncon Extra Long Life Grease is an ultra high performance lithium-complex grease with heavy synthetic base oil specifically designed for long service life under heavily loaded conditions. With an operating temperature range of -40°F to 375°F (-40°C to 191°C), this grease offers exceptional flexibility. The heavy PAO synthetic base oil and balanced antiwear and EP additives provide rock solid equipment protection day in and day out, even under heavily loaded conditions. It is fortified with antioxidant corrosion inhibitors and rust inhibitors technology. Exceptional water resistance, water washout properties and performance at nearly all temperatures make this grease an excellent choice when critical machinery is expected to work year round and in all climates. Conoco Syncon Extra Long Life Grease is specifically recommended for: Wheel bearings; Ball, roller, needle, antifriction and sleeve bearings; Gear boxes, under low speed, high loads and high temperatures; Applications where normal greases fail; Harsh, dirty, wet environments

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 155Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 2400 SUSBase Oil Property
Saybolt Viscosity at 210°F 225 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 420 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 44 cStBase Oil
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 60
Four Ball Extreme Pressure, Weld Load 315 kg
Penetration P(60), 1/10 mm 400 - 430
Timken Test 55.0 lb
 
Thermal PropertiesOriginal ValueComments
Flash Point 460 °FBase Oil Property
Dropping Point >= 500 °F
 
Descriptive Properties
Oxidation Stability3 psi drop/100 hrs
Rust Test Rating1,1,1 (Pass)
Soap Type (Thickener)Lithium Complex
Water WashoutNil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON226 / 75263

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.