Capabilities- Gauge: .005’ to .025” (126 to 635µm)
- Width: 12” to 62” (305 to 1575mm)
- Core Size: 6” standard cores, 3” and 8” available
- Roll O.D.: 29” standard, up to 40” available
- Silicone coating available
- 5 strategic manufacturing locations
Properties - Remarkable clarity
- Excellent stiffness to allow downgauging
- Superb yield
- Easily thermoformed
- FDA compliant to CFR 21 #177.1640
- Kosher Material
Information provided by Alcoa Kama Co. |
FDA Compliant: CFR 21 #177.1640 |