MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

ITW Densit® WEARFLEX 2000 Ceramic Lining
Categories: Ceramic; Oxide

Material Notes: Densit® WearFlex 2000 wear resistant linings provide superior protection against heavy erosive wear at temperatures up to 400°C (750°F).

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.90 g/cc0.105 lb/in³EN 1015-6
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity <= 70.0 GPa<= 10200 ksiDynamic; 80
Flexural Strength 20.0 MPa2900 psiEN 196-1
Compressive Strength 160 MPa23200 psiEN 12190
Abrasion 1.0 - 1.51.0 - 1.5cm3/50cm2
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C5.56 µin/in-°F
Specific Heat Capacity 0.900 - 1.00 J/g-°C0.215 - 0.239 BTU/lb-°F
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 399 °C750 °F
Shrinkage 0.20 %0.20 %Casting Shrinkage (by volume)
 
Component Elements PropertiesMetricEnglishComments
Al2O3 + TiO2 55 %55 %EN 196-10
CaO 18 %18 %EN 196-10
Fe2O3 <= 0.20 %<= 0.20 %EN 196-10
SiO2 25 %25 %EN 196-10
 
Descriptive Properties
Chromate, Cr6+ Content (%)<0.0002EN 196-10
Erosive Resistance (min/cm3)150

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWDE9084 / 239594

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.