MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Elastosil® R 752/50 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Vulcanizates made from ELASTOSIL® R 752/50 exhibit a very low rebound resilience and high damping capability.

Application: Some special applications, such as low-modulus damping elements, require silicone rubber with a particularly low impact resilience. ELASTOSIL® R 752/50 meets these requirements.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050DIN 53505
Tensile Strength at Break 8.50 MPa1230 psiDIN 53504 S1
Elongation at Break 830 %830 %DIN 53504 S1
Rebound 33 %33 %DIN 53512
Tear Strength 32.0 kN/m183 pliASTM D624 B
Compression Set 38 %
@Temperature 175 °C,
Time 79200 sec
38 %
@Temperature 347 °F,
Time 22.0 hour
DIN ISO 815-B
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
0.250 hour
@Treatment Temp. 329 °F
post cured 4h/200°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Silastic® Q7-4750 BIOMEDICAL GRADE ETR ELASTOMER, KIT
Momentive Performance Materials Addisil™ 1050 E Industrial Extrusion Heat Cured Rubber
SMAC SMACWRAP® ST Damping Material, 1 mm
Wacker Elastosil® R 401/10 Silicone Rubber
Wacker Elastosil® R plus 4000/50 Silicone Rubber

PWACK9232 / 204761

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.