MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BASF Ultramid® A 225F Natural Nylon 66, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Product Description: Ultramid® A 225F Natural is an unfilled polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles. This grade offers a good combination between primary properties of the unreinforced polyamide 66 and processing properties leading to increased productivity. These performances are associated with excellent dimensional stability and excellent filling qualities. The UL94 V2 rating at 0.4mm makes that the product is particularly used in electrical applications.

Availability: Africa & Middle East; Latin America; North America

Features: Fast Molding Cycle; Good Dimensional Stability; Good Flow; Good Mold Release

Use: Consumer Applications; Electrical/Electronic Applications; Industrial Applications; Valves/Valve Parts; White Goods & Small appliances

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Appearance: Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Maximum Moisture Content 0.20
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7250 psiISO 527-2
Tensile Strength, Yield 7250 psiASTM D638
 8700 psiISO 527-2/50
Elongation at Break 100 %ISO 527-2
 >= 200 %ASTM D638
Elongation at Yield 25 %ISO 527-2/50
Tensile Modulus 232000 psiISO 527-1
Flexural Strength 7980 psiISO 178
Flexural Modulus 203000 psiISO 178
Izod Impact, Notched (ISO) 5.70 ft-lb/in²ISO 180/A
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 4.80 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 62631-3-1
Surface Resistance 4.00e+13 ohmIEC 62631-3-2
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 509 - 527 °F
Middle Barrel Temperature 518 - 536 °F
Front Barrel Temperature 536 - 545 °F
Mold Temperature 140 - 176 °F
Drying Temperature 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2081 / 310774

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.